Bopp Heat Sealable Film
June 23, 2021
Film tertutup panas satu sisi
1.Aplikasi:
Digunakan secara luas dalam kemasan makanan & permen dll.
Ketebalan:20 μm、25μm、30 μm
Fitur:
Ø Tingkat umum
Ø Transparan, satu sisi dapat disegel panas
Ø Perawatan corona satu sisi, suhu penyegelan normal
Ø Statik rendah, ketampakan yang sangat baik, kekuatan penyegelan panas yang baik
Nilai-Nilai Tipikal:
Properti | Metode pengujian | Satuan | Nilai tipikal | ||||
Ketebalan | Kinlead | μm | 18 | 20 | 25 | 30 | |
Variasi Ketebalan | Astm-252-78 | % | ± 3.0 | ± 3.0 | ± 2.5 | ± 2.5 | |
Hasil | Kinlead | m2/kg | 61.1 | 54.9 | 44.0 | 36.6 | |
Kekuatan tarik | MD | Astm D-882 | MPa | 140 | 140 | 140 | 140 |
TD | Astm D-882 | MPa | 280 | 280 | 280 | 280 | |
Perpanjangan Pada Patah | MD | Astm D-882 | % | 175 | 175 | 175 | 175 |
TD | Astm D-882 | % | 65 | 65 | 65 | 65 | |
Koefisien gesekan | T/T-US | Astm D-1894 | - | 0.30 | 0.30 | 0.30 | 0.30 |
T/O-US | Astm D-1894 | - | 0.40 | 0.40 | 0.40 | 0.40 | |
Penyusutan Panas | MD | Astm D-1204 | % | 4.0 | 4.0 | 4.0 | 4.0 |
TD | Astm D-1204 | % | 1.5 | 1.5 | 1.5 | 1.5 | |
Kabut | Astm D-1003 | % | 1.2 | 1.5 | 1.7 | 2.0 | |
Kekuatan Penyegelan | Kinlead | N/15mm | 3.0 | 3.0 | 3.0 | 3.0 | |
Suhu Penutup | Kinlead | °C | 115 | 115 | 115 | 115 | |
Gloss | Astm D-2457 | - | 92 | 92 | 92 | 92 | |
Menghilangkan Ketegangan | Astm D-2578 | Dyn | 38 | 38 | 38 | 38 |
Nilai di atas dari sifat yang diperoleh dalam tes laboratorium kami. nilai ini untuk tujuan informatif dan tidak dalam jaminan atau jaminan dalam kondisi tertentu.Pengguna disarankan untuk melakukan pengujian sendiri untuk menentukan kesesuaian produk untuk digunakan..
Film yang dapat disegel panas dengan sisi ganda
Aplikasi:
Digunakan secara luas dalam makanan & kemasan permen ect.
Fitur:
Ø Tingkat umum
Ø Transparan, kedua sisi dapat disegel panas
Ø Perawatan corona satu sisi, suhu penyegelan normal
Ø Statik rendah, ketampakan yang sangat baik, kekuatan penyegelan panas yang baik
Ketebalan:20 μm、25μm、30 μm、40 μm、50 μm
Nilai-Nilai Tipikal:
Properti | Metode pengujian | Satuan | Nilai tipikal | |||||
Ketebalan | Kinlead | μm | 20 | 25 | 30 | 40 | 50 | |
Variasi Ketebalan | Astm-252-78 | % | ± 3.0 | ± 2.5 | ± 2.5 | ± 2.5 | ± 2.0 | |
Hasil | Kinlead | m2/kg | 54.9 | 43.9 | 36.6 | 27.5 | 22.0 | |
Kekuatan tarik | MD | Astm D-882 | MPa | 140 | 140 | 140 | 140 | 135 |
TD | Astm D-882 | MPa | 280 | 280 | 280 | 290 | 285 | |
Perpanjangan Pada Patah | MD | Astm D-882 | % | 175 | 175 | 175 | 175 | 175 |
TD | Astm D-882 | % | 65 | 65 | 65 | 65 | 65 | |
Koefisien gesekan | T/T-US | Astm D-1894 | - | 0.3 | 0.3 | 0.3 | 0.3 | 0.3 |
T/O-US | Astm D-1894 | - | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | |
Penyusutan Panas | MD | Astm D-1204 | % | 4.0 | 4.0 | 4.0 | 4.0 | 4.0 |
TD | Astm D-1204 | % | 1.5 | 1.5 | 1.5 | 1.5 | 1.5 | |
Kabut | Astm D-1003 | % | 1.5 | 1.7 | 2.0 | 2.0 | 2.2 | |
Kekuatan Penyegelan | Kinlead | N/15mm | 3.0 | 3.0 | 3.0 | 3.0 | 3.0 | |
Suhu Penutup | Kinlead | °C | 115 | 115 | 115 | 115 | 115 | |
Gloss | Astm D-2457 | - | 92 | 92 | 92 | 85 | 85 | |
Menghilangkan Ketegangan | Astm D-2578 | Dyn | 38 | 38 | 38 | 38 | 38 |
Nilai di atas dari sifat yang diperoleh dalam tes laboratorium kami. nilai ini untuk tujuan informatif dan tidak dalam jaminan atau jaminan dalam kondisi tertentu.
Pengguna disarankan untuk melakukan pengujian mereka sendiri untuk menentukan kesesuaian produk untuk digunakan.
Jika Anda ingin membeli film transparan atau film laminasi dari Cina, hanya contact me, janji tidak akan membuang-buang waktu dan harga harta karun Anda tidak akan mengecewakan Anda, tetapi melakukan dengan baik dan jangka panjang bisnis:
Whatsapp saya:008615063431351
Wechat:yuanyuan20140707